C
|
Si
|
Mn
|
P
|
S
|
0.42~0.48
|
0.17~0.37
|
0.50~0.80
|
≤0.030
|
≤0.030
|
项目
|
入炉温度/℃
|
加热温度/℃
|
开锻温度/℃
|
终锻温度/℃
|
冷却方式
|
钢锭
|
≤850
|
1150~1220
|
1100~1160
|
≥850
|
坑冷或堆冷
|
钢坯
|
1130~1200
|
1070~1150
|
≥850
|
坑冷或堆冷
|